Glass combining with PVB FILM for making laminated glass

Glass combining
Note: glass surface temperature: 20-40 ℃,
Suggest control temperature: 25-30 ℃

If temperature is higher than 40℃:
The PVB film will get shrink;
PVB film wrinkle will appear;
The film will get sealed earlier than expected;
The PVB film will get soft and adhere to the glass;
There will be lots of air inside the film.

If temperature is lower than 20 ℃:
The PVB film surface will be too smooth to get fixed;
It will be very difficult for the glass and the PVB film to get adhered;
It will be difficult to get rid of the gas and trim the edge of the
laminated glass;
There may be flaw on the edges.

All Rights Reserved By:
UCOLIN SILICONE TECH
(1)-Silicone Vacuuming Bag for EVA Glass Laminating Machine/Privacy
Glass Laminating
(2)-Silicone Sheet for EVA Glass Laminating Machine
(3)-Silicone Bag for PVB Glass Laminating Auto-clave
(4)-Silicone Rubber Sheet for Solar Cell Module Laminating Machine
(5)-Silicone Sheet for Wood Door Vacuum Laminating Machine Vacuum
Press Machine Vacuum Filming Machine
Contact Us: uc@ucolin.com / www.ucolin.com
umewe360@gmail.com/ umewe360@hotmail.com